Plastics - Unsaturated Polyester Resins - Determination Of Reactivity At 80 Degrees Celsius (conventional Method)
出版:Association Francaise de Normalisation

专家解读视频
Defines a procedure for determining the reactivity of unsaturated polyester resins characterized by the maximum temperature reached by a solution of unsaturated polyester resin and catalyst when heated in a water bath at 80 deg C, by the time taken for the temperature of the mixture to rise from 65 deg C to this maximum temperature; in addition, if the temperature is in excess of 90 deg C, by the time taken for the temperature to rise from 65 - 90 deg C. Can be used for comparison of resins of similar type.
REPLACES NFT 51-514
NEN EN ISO 584:1997 - Identical
SS EN ISO 584 Ed. 1 (1998) - Identical
UNE EN ISO 584:1998 - Identical
ISO 584:1982 - Similar
NS EN ISO 584 Ed. 1 (1998) - Identical
I.S. EN ISO 584:1998 - Identical
UNI EN ISO 584:2000 - Identical
NBN EN ISO 584:1998 - Identical
ONORM EN ISO 584:1998 - Identical
DIN EN ISO 584 (1998-03) - Identical
BS EN ISO 584:1998 - Identical
SN EN ISO 584:1998 - Identical