Aluminium And Aluminium Alloys - Anodizing - Assessment Of Resistance Of Anodic Oxidation Coatings To Cracking By Deformation
出版:Italian Standards
专家解读视频
This part describes an empirical method for assessing the resistance of anodic oxidation coatings to cracking by deformation. It is applicable particularly to sheet material with anodic oxidation coatings of thickness less than 5 micrometer, and is useful for development purposes.
NEN EN 12373-15:2000 - Identical
SS EN 12373-15 Ed. 1 (2001) - Identical
UNE EN 12373-15:2001 - Identical
NS EN 12373-15 Ed. 1 (2000) - Identical
I.S. EN 12373-15:2000 - Identical
NBN EN 12373-15:2000 - Identical
NF EN 12373-15:2000 - Identical
ONORM EN 12373-15:2000 - Identical
DIN EN 12373-15 (2000-12) - Identical
BS EN 12373-15:2001 - Identical
SN EN 12373-15:2000 - Identical