Vitreous and porcelain enamels — Low-voltage test for detecting and locating defects — Part 2: Slurry test for profiled surfaces
出版:International Organization for Standardization

专家解读视频
This document specifies a low-voltage test method for detecting and locating defects (pores, cracks or pop-offs) that occur in enamel coatings of corrugated and/or undulated profiles and that extend down to the metal base.
UNI EN ISO 8289-2:2019 - Identical
SS-EN ISO 8289-2:2019 - Identical
PN-EN ISO 8289-2:2019-06 - Identical
EN ISO 8289-2:2019 - Identical
I.S. EN ISO 8289-2:2019 - Identical
BS EN ISO 8289-2 : 2019 - Identical
DS/ISO 8289-2:2019 - Identical
DS/EN ISO 8289-2:2019 - Identical
?NORM EN ISO 8289-2:2019 - Identical
NS-EN ISO 8289-2:2019 - Identical
PN-EN ISO 8289-2:2019-06 - Identical
UNI EN ISO 8289-2:2019 - Identical
EN ISO 8289-2:2019 - Identical
NS-EN ISO 8289-2:2019 - Identical
I.S. EN ISO 8289-2:2019 - Identical
DS/ISO 8289-2:2019 - Identical
?NORM EN ISO 8289-2:2019 - Identical
DS/EN ISO 8289-2:2019 - Identical
BS EN ISO 8289-2 : 2019 - Identical
SS-EN ISO 8289-2:2019 - Identical