Specifications For Particular Types Of Winding Wires - Part 0-4: General Requirements - Glass-fibre Wound, Resin Or Varnish Impregnated, Bare Or Enamelled Rectangular Copper Wire
出版:German Institute for Standardisation (Deutsches Institut für Normung)

专家解读视频
Specifies the general requirements of glass-fibre wound bare and of glass-fibre wound enamelled rectangular copper winding wires. Coverage includes dimensions, heat shock, loss of mass, elongation, breakdown voltage, temperature index, solderability, electrical resistance, resistance to solvents, and packaging. Also includes annexes and tables.
Supersedes DIN IEC 60317-0-4. (05/2002) DRAFT 2014 issued in August 2014. (08/2014)
UNE EN 60317-0-4:1999 - Identical
SS EN 60317-0-4:1998 - Identical
NF EN 60317-0-4:2000 - Identical
EN 60317-0-4:2016 - Identical
NF EN 60317-0-4:2016 - Identical
SN EN 60317-0-4:2016 - Identical
BS EN 60317-0-4:2016 - Identical
SN EN 60317-0-4:1998 - Identical
BS EN 60317-0-4:1998 - Identical
IEC 60317-0-4 Ed. 2.2 - Identical
I.S. EN 60317-0-4:1998 - Identical