ALUMINIUM OXIDE PRIMARILY USE FOR THE PRODUCTION OF ALUMINIUM - DETERMINATION OF LOSS OF MASS AT 300 DEGREES C AND 1000 DEGREES C
出版:International Organization for Standardization

专家解读视频
Provides a method for the determination of loss of mass on heating of aluminium oxide at 300 degrees C and further loss of mass on ignition at 1000 degrees C.
NBN T 03 405 : 1983 - Identical
BS 4140-3(1986) : 1986 - Identical
BS ISO 806 : 2004 - Identical
NEN ISO 806 : 2004 - Identical
NEN ISO 806 : 2004 - Identical
BS ISO 806 : 2004 - Identical